Solder Defects

Tin bath in float glass is melted glass melting furnaces under the system of liquid at a certain temperature, through the main drive and pull the edge of the external force, a certain width thickness glass, after cooling through the transition rollers into the annealing Lehr.

Tin bath of float process uses metal tin as a floating support medium, nitrogen gas and hydrogen gas mixture as protection. In a tin bath in this relatively confined environment, undergoing many complex chemical reactions, some of these chemical products will bring a lot of glass defects, affect the quality of the product.

Tin bath in float glass environment and structural characteristics of solder defects is inevitable, can only be effectively controlled in the actual production, not eliminate it.